Choosing pre-galvanised vs hot-dip galvanised strut, or stepping up to stainless, decides how long a support system lasts. Under-specify and the containment corrodes before the cables are due for replacement. Over-specify and you pay for stainless in a dry office riser. This guide compares the finishes with coating thicknesses, corrosivity classes and a simple life calculation.
Pre-galvanising, also known as the Sendzimir process, coats steel strip continuously in a zinc bath before it is rolled into channel. The coating is specified to BS EN 10346 [1]. Because the channel is punched and cut afterwards, those edges carry no zinc of their own.
How do pre-galv, HDG and zinc plating compare?
| Property | Pre-galvanised (PG) | Hot-dip galvanised (HDG) | Electro-galvanised (EG) |
|---|---|---|---|
| When coated | As strip, before forming | As a finished product, after forming | As a part, by electroplating |
| Coating | Per Z grade; Z275 is about 20 µm per side | 45–55 µm on strut, 60–70 µm on ladder | Thin, a few µm |
| Edges and slots | Bare | Coated | Coated |
| Standard | BS EN 10346 [1] | BS EN ISO 1461 [2] | ISO 2081 [3] |
| Typical use | Indoors, dry | Outdoors, damp, industrial | Small parts, indoors |
HDG thickness: manufacturer data [6]. Z275: calculated from 275 g/m² over both faces at a zinc density of 7.14 g/cm³. Electro-galvanised: rule of thumb, indicative. Your supplier confirms the actual coating.
The 45 to 55 µm on hot-dip galvanised strut is consistent with BS EN ISO 1461, which asks for a mean coating of at least 55 µm on steel from 1.5 to 3 mm thick [2]. Cable ladder uses thicker steel and so picks up a heavier coat.
How long does a zinc coating last?
Zinc corrodes at a rate set by the atmosphere. ISO 9223 gives a first-year range for each corrosivity class [4]. Divide the coating thickness by that rate and you get a rough life to first maintenance.
| Class | Zinc loss (µm/year) | Pre-galv, about 20 µm (years) | HDG, 55 µm (years) |
|---|---|---|---|
| C1 very low | ≤ 0.1 | > 100 | > 100 |
| C2 low | 0.1–0.7 | ≥ 29 | ≥ 79 |
| C3 medium | 0.7–2.1 | 10–29 | 26–79 |
| C4 high | 2.1–4.2 | 5–10 | 13–26 |
| C5 very high | 4.2–8.4 | 2–5 | 7–13 |
| CX extreme | 8.4–25 | 1–2 | 2–7 |
Corrosion rate: ISO 9223 [4]. Life: worked example, indicative. Real rates often slow after the first year, while edges and damage go first.
The pattern is clear. In a dry indoor space, pre-galv is more than enough. From C3 upwards HDG wins comfortably, and in C5 or CX stainless takes over.
Which corrosivity class is your location?
| Class | Indoor examples | Outdoor examples | Finish (rule of thumb) |
|---|---|---|---|
| C1 | Heated offices, schools, dry plant rooms | n/a | Pre-galvanised |
| C2 | Unheated stores, sports halls, occasional condensation | Rural, low pollution | Pre-galv indoors, HDG outdoors |
| C3 | Humid production: food processing, laundries, breweries | Urban and light industrial, low-salinity coast | HDG |
| C4 | Chemical plants, swimming pools | Industrial, moderate-salinity coast | HDG or stainless 316 |
| C5 | Near-permanent condensation and pollution | Humid industrial, high-salinity coast | Stainless 316 |
| CX | Extreme humidity and aggressive atmosphere | Offshore | Stainless 316 or a special alloy |
Examples per BS EN ISO 12944-2 [5]. Finish: rule of thumb, indicative; if in doubt, measure the class on site.
UK sites near the coast deserve a second look. A plant room on an estuary can sit a class higher than the building next to it inland.
When should you specify 304 or 316 stainless?
Grade 304 (1.4301) handles moisture and most clean environments. Grade 316 (1.4401 or 1.4404) contains molybdenum and copes far better with chlorides, which come from sea air, salt water, pool atmospheres and many cleaning agents.
- Food and pharma: 316. Stainless 316 cable basket and open channel are easy to wash down and tolerate the chemicals. See food and pharma.
- Swimming pools: ask the manufacturer. For load-bearing parts in indoor pool atmospheres, BS EN 1993-1-4 sets extra requirements on the stainless grade [7].
- Stainless with stainless. In stainless channel, use stainless channel nuts, bolts and rod: A4 with 316. Keep stainless away from galvanised steel in wet locations, or fit a plastic isolator.
What should you do with cut edges and damage?
Every cut is a spot without zinc. On pre-galv in a dry space, the surrounding zinc usually protects a thin edge well enough (rule of thumb, indicative). In damp areas and on HDG work, touch up every cut and scratch with zinc-rich paint.
Storage matters too. Galvanised steel left wet without airflow develops white rust, a white bloom of zinc salts. Store channel dry and ventilated, with battens between layers. Light white rust is mostly cosmetic; heavy deposits warrant a thickness check.
Welding galvanised steel releases zinc fume and needs extraction. With bolted strut, you can avoid welding altogether.
Where does aluminium fit?
Aluminium is light, non-magnetic and resists corrosion well in many atmospheres. You see it mostly as cable ladder over racks in data centres and in marine work. It is less stiff than steel, so spans get shorter. Separate aluminium from galvanised or stainless steel in damp conditions to prevent galvanic corrosion.
How does the configurator suggest a finish?
Every configuration starts with “Application and environment”: sector, location and atmosphere. The configurator then proposes a finish, which you can override:
| Situation | Proposed finish |
|---|---|
| Indoors and dry, including data centres | Pre-galvanised |
| Outdoors or on a roof | Hot-dip galvanised |
| Hygienic, food and pharma | Stainless 316 |
| Marine and offshore | Stainless 316 |
| Aggressive | Hot-dip galvanised; stainless 316 in industry |
Configurator defaults, based on the tables above. The manufacturer’s advice prevails.
If the project needs circuit integrity in a fire, the configurator flags it. The finish alone does not answer that; the manufacturer’s tested assembly does.
Where do these figures come from?
- BS EN 10346, Continuously hot-dip coated steel flat products for cold forming, technical delivery conditions (Z grades).
- BS EN ISO 1461, Hot dip galvanized coatings on fabricated iron and steel articles, specifications and test methods.
- ISO 2081, Metallic and other inorganic coatings, electroplated coatings of zinc with supplementary treatments on iron or steel.
- ISO 9223, Corrosion of metals and alloys, corrosivity of atmospheres, classification, determination and estimation (zinc corrosion rate per class).
- BS EN ISO 12944-2, Paints and varnishes, corrosion protection of steel structures by protective paint systems, Part 2: Classification of environments.
- Eurostrut, product descriptions for hot-dip galvanised strut (45 to 55 µm) and ECL cable ladder (60 to 70 µm). Accessed 19-11-2026. https://eurostrut.com/montageprofiel-41x41mm-met-gaten-3m-tv/ES1000THDG3M · https://eurostrut.com/kabelladder-ecl100-1000mm-tv/ECL100-1000-6-HDG
- BS EN 1993-1-4, Eurocode 3: Design of steel structures, Part 1-4: Supplementary rules for stainless steels (annex on selecting the grade).
- Atkore UK, P1000 channel finishes PG, HG and SS. Accessed 19-11-2026. https://www.atkore.com/en-gb/products/metal-framing-and-fittings/P1000
Frequently asked questions
Is pre-galvanised steel suitable for outdoor use?
Generally not for long. Outdoors you are quickly in corrosivity class C3 or higher. A simple calculation puts a zinc layer of about 20 µm at 10 to 29 years in C3, and cut edges rust sooner. Specify hot-dip galvanised or stainless outdoors.
What is the difference between pre-galv and HDG?
Pre-galvanised steel is coated as strip before it is formed, so the zinc is thinner and punched or cut edges are bare. Hot-dip galvanised products are dipped after forming, covering edges and slots too. On strut channel that gives 45 to 55 µm of zinc.
When do I need 316 rather than 304 stainless?
Wherever chlorides are present: sea air, salt water, swimming pool atmospheres and many cleaning chemicals. Grade 316 contains molybdenum, which improves resistance to pitting. In food and pharmaceutical plants, 316 is the usual choice for washable support systems.
Can I mix stainless fixings with galvanised channel?
Avoid it in wet locations. Stainless in contact with zinc in the presence of moisture drives galvanic corrosion of the zinc. Keep systems consistent, A4 fixings in 316 channel and galvanised fixings in galvanised channel, or separate them with a plastic isolator.
https://strutconfigurator-site.pages.dev/en/knowledge-base/pre-galvanised-vs-hot-dip-galvanised-vs-stainless/ · Updated 19 November 2026 · Indicative; the manufacturer confirms.